Anti glare coatings
Kriya offers anti glare coatings with adjustable haze levels, applicable in among others displays where high transparency is a must. The anti glare functionality can be combined with other properties to make it multi-functional.
The anti glare coating technology is applicable for glass and plastic substrates as shown below.
Anti glare glass coating
This coating combines light diffusion with the highest transmission and lowest optical clarity. The coating is:
√ Inorganic
√ Solvent based
√ Thermal curable
The glass anti glare level (gloss, haze and clarity) can be custom formulated upon request.
Typical applications are: agricultural greenhouses and OLED & LED lights. Possible Gloss 60° (GU units), haze tunable as high as 90% for glass, clarity as low as 10%.
Anti glare and anti scratch coating for plastics
The Anti glare scratch resistant hard coat is a protective light diffusing coating for transparent substrates. This product is developed mainly for plastic sheets and roll-to-roll film such as PET, TAC, PC, PMMA and others.
Our coatings are standard available as a solvent based, UV curable organic/inorganic hybrid which offers high transparency and scratch resistance to the substrate.
The anti glare level (gloss, haze) is custom formulated upon request and includes standard products such as AG-3. AG-8 and AG-25 with low sparkling at 400 PPI.
Typical applications are: display coatings.
Available gloss levels and added features are shown in the tables below.
| Type | PET | TAC | PC | PMMA | Glass |
|---|---|---|---|---|---|
| Organic | 50-160 | 50-160 | 15-160 | 15-160 | * |
| Inorganic | * | * | * | * | 5-160 |
* = Optional additional feature
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.
| Type | Scratch resistance | Overcoatable | Chemical resistance | Anti static |
|---|---|---|---|---|
| Organic | V | * | * | * |
| Inorganic | V | * | * | * |
V = Standard | * = Optional additional feature
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.