Anti-scratch hard coating
Kriya Material’s anti-scratch coating is a clear coating which provides a durable and scratch resistant functionality to a large range of plastic surfaces. This coating is available for among others:
√ Polethylene terephtalate (PET)
√ Triacetate cellulose (TAC)
√ Polycarbonate (PC)
√ Polymethylmethacrylate (PMMA)
√ Cyclo Olefin Polymers (COP)
√ Polyamide (PA6)
√ Polyimide (CPI and TPI)
√ Thermoplastic polyurethane (TPU)
√ Polyvinylchloride (PVC)
√ Acrylonitrile butadiene styrene (ABS)
√ Styrene acrylonitrile (SAN)
but not limited to other substrates l. Due to our in-house experience, we can adapt and fine tune the formulations to both your technical requirements and industrial processing conditions.
Characteristics
Standard properties of our anti-scratch coating are high transmission, low haze, high clarity and provide excellent adhesion to the substrate. Upon request, properties such as chemical resistance, hydrophilicity and overcoat ability can be added. The combination with functionalities such as anti-static, anti-glare, anti-fouling/hydrophobic, etc are possible in one single layer.
The above properties and functionalities can be realized in a dry coating layer thickness between 2 and 10 µm, depending on the substrate, mechanical requirements and processing conditions.
Typical applications of this coating are: protective films, in- cartainment, touch panels, digital signage, screen protection, polarizer films, displays.
Hard coats
The scratch resistant hard coat is a protective coating for transparent substrates. This product is developed mainly for plastic sheet and roll-to-roll film coating such as PET, TAC, PC, PMMA and others. Our products are standard available as a solvent based, UV curable organic/inorganic hybrid which offers high optical transparency and scratch resistance to the substrate. For glass and steel, it is a solvent based inorganic system which is applied as a primer for subsequent functional layers as well as top coat for the improvement of scratch resistance and durability of the surface.
Pencil Hardness measured according to the Wolf Wilburn principle with 750gr. loading
| Type | PET | TAC | PC | PMMA | Glass | STEEL ETC. |
|---|---|---|---|---|---|---|
| Organic | 4H | 3H | H | 6H | * | With primer |
| Inorganic | * | * | * | * | 9H | 9H |
* = Optional additional feature
| Type | Scratch resistance | Overcoatable | Chemical resistance | Anti static |
|---|---|---|---|---|
| Organic | V | * | * | * |
| Inorganic | V | * | * | * |
V = Standard | * = Optional additional feature
Best in class performance
At Kriya Materials you are assured of a custom specific coating. Meeting your most stringent requirements is our goal. We create a coating with an optimal performance at the lowest possible system cost. Do you have specific needs? No problem! As an innovative organization we love to think along! Contact us and share your technical requirements as much as possible. Please check our development process and get inspired.