OLED and LED Lights – Hydrophilic (Anti fog)
Kriya hydrophilic coating is a solvent based, thermal curable coating for glass. Next to its excellent optical clarity, it combines a low water contact angle and outstanding Light stability. Furthermore, it has an antistatic functionality improving static discharge of a surface.
| Type | PET | TAC | PC | PMMA | Glass | Steel etc. |
|---|---|---|---|---|---|---|
| Organic | WCA ‹15 | WCA ‹15 | WCA ‹15 | WCA ‹15 | ||
| Inorganic | WCA ‹15 | WCA ‹15 |
0 = Standard | X = Optional additional feature
| Type | Scratch resistance | Overcoatable | Chemical resistance | Anti static | Near Infra Red |
|---|---|---|---|---|---|
| Organic | 0 | X | X | ||
| Inorganic | 0 | X | X |
0 = Standard | X = Optional additional feature
Kriya Materials if needed develops custom formulations meeting the most stringent requirements of our customers. The result is a plug and play product designed for optimal performance at the lowest total system cost.
Please contact us through submitting our intake form.
Coatings for other substrates can be requested @ Kriya Materials
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.