Display coatings – Antistatic hardcoats
The Antistatic hard coat is a solvent based UV curable coating. It combines high transparency, low haze and hard coat properties. The conductivity of the coating can be tuned from E+06 to E+10 depending on the transmission and hardness requirements. For plastics such as PET, TAC, PC, PMMA etc, we can offer either a solvent based, UV curable organic/inorganic hybrid or a water based, thermal curable hybrid. For glass, it is a solvent based inorganic system for which the surface resistance can achieve values as low as 1 MΩ/□, when properly sintered.
Uncoated PC lense
PC lense coated with an antistatic HC
Achievable Surface resistivity in Ω/□, measured with a ring electrode at 999V. Lower resistance available upon request.
Type | PET | TAC | PC | PMMA | Glass |
---|---|---|---|---|---|
Organic | 10E+06 | 10+E06 | 10E+06 | 10E+06 | X |
Inorganic | X | X | X | X | 10E+06 |
0 = Standard | X = Optional additional feature
Type | Scratch resistance | Overcoatable | Chemical resistance |
---|---|---|---|
Organic | 0 | X | X |
Inorganic | 0 | X | X |
0 = Standard | X = Optional additional feature
Kriya Materials always develops custom formulations meeting the most stringent requirements of our customers. The result is a plug and play product designed for optimal performance at the lowest total system cost.
Since we work custom based, we love to hear more about your substrate of interest and envisioned functionalities.
Please contact us through submitting our intake form.
Coatings for other substrates can be requested @ Kriya Materials
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.