All products
KM-105100% PFAS-free

Thermal LRI

Thermal-curable low refractive index coating reaching RI 1.16. Overcoatable and PFAS-free. Survives tempering at 630°C on glass. Delivers up to 3.9% transmission gain and 4.5× light guiding luminance improvement.

Refractive index rangen = 1.161.40
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-101–140

Specifications

Functions

Low RIAnti-reflective

Compatible substrates

GlassPET

Processing methods

SPINDIPSPRAY

Refractive index range

1.161.40
1.162.00
PropertyValue
Product codeKM-105
Chemistry familySolvent sol-gel
Refractive index range1.161.40
Cure typeThermal
PFAS status100% PFAS-free
FunctionsLow RI, Anti-reflective
Compatible substratesGlass, PET
ProcessingSPIN, DIP, SPRAY
Product blockKM-101–140
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us