Displays & wearables

WOLED TV panel

White OLED with colour filters, light out through the glass

Large OLED TVs use white OLED emitters with colour filters and send the light out through the TFT glass (bottom emission). Much of it never gets out: in bottom-emission OLEDs about half of the emitted light stays trapped in, or is absorbed by, the anode and organic layers, and more is trapped in the glass. A high-index extraction layer between electrode and substrate passes part of the trapped light into the glass; a low-reflection coating on the front keeps room light from lifting the blacks.

VIEWER SIDEBACK COVERLow-reflection AR, hard coat,easy-cleanOn the front polarizer filmCircular polarizerNot KriyaTFT glass substrateLight exits here · n 1.52TFT arrayNot KriyaColour filters on the arrayRed, green, blue (plus white)Internal light-extraction layerHigh-index nanoparticle layer with a flatsurfaceTransparent anode (ITO)n ≈ 2.0White OLED stackTandem emitters · n ≈ 1.75Reflective cathodeNot KriyaEncapsulation and back coverNot KriyaK1K2
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (10)
  1. Low-reflection AR, hard coat, easy-clean On the front polarizer filmK1
  2. Circular polarizer Not Kriya
  3. TFT glass substrate Light exits here · n 1.52
  4. TFT array Not Kriya
  5. Colour filters on the array Red, green, blue (plus white)
  6. Internal light-extraction layer High-index nanoparticle layer with a flat surfaceK2
  7. Transparent anode (ITO) n ≈ 2.0
  8. White OLED stack Tandem emitters · n ≈ 1.75
  9. Reflective cathode Not Kriya
  10. Encapsulation and back cover Not Kriya

Public references

  1. K. Saxena, V. K. Jain, D. S. Mehta, A review on the light extraction techniques in organic electroluminescent devices — Opt. Mater. 32, 221 (2009): light out-coupling techniques, among them scattering media and substrate modification
  2. US 9,147,856 — Organic light emitting device — internal extraction can in theory raise efficiency more than about three times; an attached micro-lens array gives about 50 %

Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.