Displays & wearables
Smartwatch
Display cover and optical heart-rate sensor
A smartwatch has two optical windows. The cover over the display has to stay readable in full sun; the rear window lets green, red and infrared LEDs measure blood flow in the skin (photoplethysmography, PPG). Both lose light at every surface — bare sapphire reflects 7.7 % per surface, glass 4.3 %.
Kriya coating position — published on kriya-materials.comKriya chemistry applies — application fit from public literatureOther device layers — not supplied by Kriya
All layers (11)
- Easy-clean topcoat Fluorine-free optionK1
- Anti-reflection coating Single low-index layer or multi-layer ARK2
- Cover crystal Sapphire (n 1.77) or strengthened glass (n ≈ 1.5)
- Optically clear adhesive Not Kriya
- Circular polarizer Not Kriya
- Touch sensor Not Kriya
- OLED display LTPO OLED
- Case, battery and electronics Not Kriya
- Sensor board Green, red and infrared LEDs, photodiodes
- Light barriers and Fresnel lenses Block LED-to-detector crosstalk, shape the beams
- Rear sensor window Sapphire, glass or polymer lenses · skin side
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.