Prescription spectacle lens
A prescription lens is a soft plastic that needs a hard coat, and most lenses also carry an anti-reflection stack and an easy-clean top layer. The hard coat is a few micrometres thick. If its index differs from the lens, light reflected at the hidden boundary between them interferes with the surface reflection and the lens shows rainbow-like fringes — worse the higher the lens index. Matching the hard coat's index to the lens removes the boundary optically.
All layers (7)
- Easy-clean topcoat FrontK4
- Anti-reflection stack FrontK3
- Index-matched hard coat 1–5 µm · antistatic optionK1 · K2
- Lens ADC n 1.50 · polycarbonate 1.59 · polythiourethane 1.60 and 1.67 · episulfide 1.74
- Index-matched hard coat BackK1 · K2
- Anti-reflection stack BackK3
- Easy-clean topcoat BackK4
Working method
Version 1 · first publishedA hard coat with the index of the lens, a wet-coated AR stack on top, an easy-clean layer to finish.
Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.
- Hard coat with the index of the lens
Solvent-free, index up to 1.65: matches polycarbonate and n 1.60 lenses and cuts the swing on n 1.67 to 5.7–6.3 %. Antistatic option: 10⁶–10¹² Ω/sq.
Layers: Index-matched hard coat - Wet-coated AR on the hard coat
Thin-film model: quarter-wave n 1.30 (106 nm) on half-wave n 1.95 (141 nm) on quarter-wave n ≈ 1.6 (about 85 nm), below 0.05 % luminous reflectance. Kriya's published value for multi-layer AR: R < 0.15 %.
Layers: Anti-reflection stack - Easy-clean top layer
Water contact angle above 100° without fluorinated chemistry.
Layers: Easy-clean topcoat
Public basis
Earlier public documents that describe the same steps.
- US 5,165,992 — Hard coating film and optical elements having such coating film — 1991: high-index oxide particles in the hard coat suppress interference fringes on n 1.56 and n 1.60 lenses.
- US 8,432,624 — Optical article and method for producing the same — Its background records oxide nanoparticles in the hard coat as the way to raise its index.
- US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998: UV-curable transparent coating made antistatic with conductive tin-oxide powder, on substrates such as polycarbonate.
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — Textbook: three-layer anti-reflection designs for the visible with a half-wave layer in the middle.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Stays with the device maker
Lens material, surfacing and tint.
A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.
Public references
- US 8,432,624 — Optical article and method for producing the same — fringes from index mismatch and thickness variation on n 1.67 and 1.74 lenses; oven cure at 125 °C
- US 5,165,992 — Hard coating film and optical elements having such coating film — 1991 filing: high-index oxide particles in the hard coat suppress interference fringes on high-index plastic lenses
- US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.