AR glasses — holographic waveguide
A holographic waveguide couples light in and out with volume gratings recorded in a photopolymer or liquid-crystal layer only a few micrometres thick. The substrates around it can be thin glass or plastic of ordinary index, so the range of guided angles is narrow from the start. Every layer added outside the guide — a cover, a second colour plate, a laminate — has to be separated from it by something of very low index.
All layers (9)
- Hard coat, AR and easy-clean On the world-side coverK1
- World-side cover Bonded with optical adhesive · not Kriya
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Substrate Glass or polymer, 50–500 µm · n ≈ 1.52
- Holographic grating layer Photopolymer or liquid-crystal polymer, 2–5 µm · not Kriya
- Substrate Glass or polymer
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Eye-side cover plate Bonded with optical adhesive · not Kriya
- Hard coat and multi-layer AR Eye sideK1
Working method
Version 1 · first publishedA low-index layer on both outer faces of the guide, flat covers bonded over it, coated outer faces.
Step by step: where each layer goes, its index, its thickness and how it is cured. Compositions are not part of it. Point at a step to see its layers.
- Coat both outer faces of the guide with a low-index layer
n about 1.2, 0.5–2 µm. Against n 1.20 an n 1.52 guide guides beyond 52.1°. For polymer substrates: n 1.21 with an 80 °C cure, UV-curable from n 1.30.
Layers: Low-index layer - Bond flat covers over it
Optical adhesive on the low-index layer. Adhesive and covers are not Kriya.
Layers: World-side cover · Eye-side cover plate - Coat the outer faces
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.
Layers: Hard coat, AR and easy-clean · Hard coat and multi-layer AR
Public basis
Earlier public documents that describe the same steps.
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000: a layer bonded to a light guide through a lower-index layer; guided light is totally reflected at that interface.
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001: a low-index coating made of fine hollow particles in a binder.
Stays with the device maker
The grating layer, its recording and the layout of the guide.
A working method describes how a coating can be applied. It is not legal advice. The design of a complete device, and clearing it against the rights of others, stays with the device maker.
Public references
- B. Kress, Optical waveguide combiners for AR headsets: features and limitations — Proc. SPIE 11062, 110620J (2019)
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
More on kriya-materials.com
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.