A thin film reflects light from both its interfaces. The two reflected waves interfere. The condition for destructive interference at normal incidence — where the two waves cancel — is that the round-trip optical path length through the film equal half a wavelength.
n · d is the film’s optical thickness: physical thickness scaled by the refractive index. For a film meant to reflect light at 550 nm (green), the quarter-wave condition fixes nd = 137.5 nm.
Why both interfaces, both phase-flipped
Reflection off a boundary toward higher index picks up a π phase flip; reflection off a boundary toward lower index does not. An air → film → glass stack with nfilm > nair and nfilm < nglass flips both. The round trip inside the film adds another 2·(2π/λ)·nd, so destructive interference lands at nd = λ/4.