Refractive index and dispersion

What n means, how it moves with wavelength, where k enters.

Lesson 1 of 5 · ~8 min read

The refractive index n of a medium is the ratio of the speed of light in vacuum to its phase velocity in the medium. For transparent dielectrics in the visible range it carries almost all the physics you need to design a coating: reflection, refraction, interference, and — in the right range of thicknesses — colour.

n is complex

For media that absorb, we write the complex refractive index as

nc = n − i k,

where k is the extinction coefficient. We use the physics sign convention (nc = n − i k, k ≥ 0) throughout the Kriya tools and this course; it matches Born & Wolf and Hecht. Weak dielectrics have k ≈ 0 across the visible; metals have k of order unity.

n depends on wavelength

In the normal-dispersion regime away from strong absorptions, n(λ) decreases with wavelength. A few points of reference at 550 nm:

  • Air: 1.000
  • Water: 1.333
  • PMMA: 1.491
  • BK7 glass: 1.517
  • Polycarbonate (PC): 1.585
  • PET (biaxial): 1.65–1.66
  • Silicon: 3.48 (weakly absorbing in the visible)