At normal incidence (the light beam hits the surface perpendicular, θi = 0°) the two polarisations are identical and the Fresnel equations collapse to one compact formula.
R0 = ((n1 − n2) / (n1 + n2))2
(2.1)
Three consequences that come up in every design review:
- No contrast, no reflection. If n1 = n2, R0 = 0. This is the physical basis of index-matching fluids and the reason a lamination that matches indices perfectly is invisible.
- 4% at every air/glass surface. For air (1.00) → BK7 (1.52), R0 ≈ 4.26%. A bare glass slab reflects 4% off the front and ~4% off the back, so ~8% total. This 8% is the number every AR coating is trying to cancel.
- Reciprocity. The formula is symmetric in n1 and n2. Light going from glass into air reflects with the same R0 as light going from air into glass.