Hands-on exercises

Three short tasks in the Light Guide Plate Simulator. Each one gives you the inputs; you report the number.

This tool doesn’t accept URL parameters, so the “Open in tool” buttons below open the tool at its landing page. Set the inputs listed in each exercise by hand.

PMMA against air — guided fraction

Compute the baseline guided fraction for a bare-air PMMA plate.

Inputs to set
  • n_plate: 1.49 (PMMA)
  • n_outside: 1.00 (air)
  • Return guided fraction (%)
Open in tool ↗Open the Light Guide Plate Simulator. Set the plate to PMMA (n = 1.49) with air on both faces. Record the guided fraction.

PMMA with a 1.20 cladding

Add a low-index cladding and compare.

Inputs to set
  • n_plate: 1.49 (PMMA)
  • n_cladding: 1.20
  • Return guided fraction (%)
Open in tool ↗Keep PMMA; replace the air with a 1.20 cladding on both faces. Record the guided fraction.

AR on the PMMA top surface

Compute the top-surface reflectance with a quarter-wave MgF₂ AR.

Inputs to set
  • Film: MgF₂, n = 1.38
  • Thickness: 550/(4·1.38) nm
  • Substrate: PMMA, n = 1.49
  • λ = 550 nm
Open in tool ↗Apply a quarter-wave MgF₂ (n = 1.38) AR coating to the top of a PMMA plate at 550 nm. Record R.