Hollow-sphere geometry

Outer radius, shell thickness, void fraction — the three numbers that set the particle index.

Lesson 1 of 5 · ~7 min read

A hollow sphere is described by three numbers: outer diameter D, shell thickness t, and the shell material's refractive index nshell. The core is usually air, ncore = 1.00. Everything about the particle's optical response — its effective index, how it mixes into a binder, how it scatters — flows from those three.

The two radii

router = D/2, rinner = router − t

The core radius must stay positive, so the shell thickness has a hard upper bound at D/2. In practice it is well below that — thin shells are the whole point.

Void fraction

φvoid = Vinner / Vouter = (rinner/router)³

A 100 nm particle with a 10 nm silica shell is 51.2 % air by volume (inner radius 40 vs outer radius 50, (40/50)³). Halve the shell to 5 nm and that jumps to 72.9 % ((45/50)³). The void fraction is what the effective-medium step turns into an index.

Low-refractive-index coatings down to RI 1.16, overcoatable and PFAS-free, live on the low-refractive-index-coatings technology page.