Hold a clear glass panel at an angle under a bright lamp and you see the lamp twice. The first reflection comes off the front surface. The second — fainter, offset, often slightly different in colour — is a ghost: light that passed into the glass, reflected off the back surface, and came back out through the front.
The double-bounce path
Ghost Lab treats the panel as four interfaces along one ray: air → coating stack → glass → back-surface stack → air. For an uncoated slab that collapses to two Fresnel surfaces separated by the substrate. The ghost ray is the one that transmits through the front, reflects off the back, and transmits out through the front again — three Fresnel events that each take a small bite out of the amplitude.
Both front transmittances are close to 1 — you lose at most a few percent on a bare glass front — so the ghost's brightness is dominated by the product Rfront · Rback, which we use as the working expression throughout the module. We ignore the double-bounce inside the slab (back → front → back → out); it is of order R3 and lands two orders of magnitude below the first ghost.
Why the ghost is offset
The two images are not on top of each other because the ghost ray refracts into the glass, travels sideways through a slab of thickness d, reflects, and travels back out. The lateral shift on the glass surface is
where θt is the refracted angle inside the glass (Snell: sin θt = sin θi / n). For a 1 mm BK7 slab viewed at 30° in air, θt ≈ 19.2°, giving Δx ≈ 0.70 mm on the glass surface — enough that an eye focused on the front sees a visibly separate second image of any small bright source.