Low refractive index coatings
Kriya’s Low Refractive Index (LRI) coating is a solvent based, UV curable coating with a tuneable refractive index (RI) as low as 1.35 for polymeric substrates or optionally available as an inorganic thermal curable coating for glass. It is one of the few PFAS free coatings with this low refractive index available worldwide. It can be used in optical stacks to match the RI requirements in that specific construction. It is frequently used to reduce the reflection of a plastic substrate up to a certain extent, or as part of a waveguide structure to guide light into a specific direction. In combination with a Kriya’s hard coat or Antistatic hard coat as a base layer it is possible to add properties such as additional mechanical and/or antistatic properties. The LRI coating can be applied by standard wet coating techniques such as gravure and slot die, and in combination with the High refractive index layers as offered by Kriya sophisticated anti-reflection coatings can be made.
Type | PET | TAC | PC | PMMA | Glass |
---|---|---|---|---|---|
Organic | Min 1.35 | Min 1.35 | Min 1.35 | Min 1.35 | |
Inorganic | Min 1.35 |
0 = Standard | X = Optional additional feature
Type | Scratch resistance | Overcoatable | Chemical resistance | Antistatic |
---|---|---|---|---|
Organic | separate layer | X | X | separate layer |
Inorganic | separate layer | X | X | separate layer |
0 = Standard | X = Optional additional feature
Kriya Materials always develops custom formulations meeting the most stringent requirements of our customers. The result is a plug and play product designed for optimal performance at the lowest total system cost.
Since we work custom based, we love to hear more about your substrate of interest and envisioned functionalities.
Please contact us through submitting our intake form.
Coatings for other substrates can be requested @ Kriya Materials
Disclaimer; Performance may depend on specific subtrate of choice, and process conditions, for each customer a customer specific product is formulated.