Swanepoel Envelope Analyzer
How do I extract refractive index and thickness from a transmission spectrum?
Extract refractive index n(λ), extinction coefficient k(λ), and physical thickness d from a coated-film transmission spectrum plus a bare-substrate reference, including a closed-form low-index (n < s) branch derived in-house for porous-silica LRI coatings.
How it works
The Swanepoel envelope method fits two smooth curves to the maxima and minima of a transmission spectrum through a thin film on a transparent substrate. The ratio and separation of the envelopes give the refractive index and the thickness; the absorption coefficient follows from the envelope average. The result depends only on the spectrum and the substrate index.
Worked example
a-Si:H envelope from Swanepoel 1983 Table 1
Transmission envelope → thickness, n(λ) via Swanepoel 1983.
Validation method, references and test-case results: /validation#swanepoel