Mie Scattering

How do nanoparticles of this size scatter visible light?

Nanoparticle extinction. Compute scattering, absorption, and extinction efficiency factors for a nanoparticle dispersion using Mie's 1908 exact solution to Maxwell's equations. Transmittance through a filled layer via Beer-Lambert. For Kriya TiO₂, ZrO₂, SiO₂, Al₂O₃ dispersions in solvent, polymer binder, or Kriya LRI/HRI.

How it works

Mie theory gives the exact scattering and absorption cross sections of a homogeneous sphere illuminated by a plane wave, as functions of the size parameter and the complex refractive indices of sphere and host. In the small-size limit it reduces to Rayleigh scattering; around the size parameter of unity, resonances in the scattering phase function dominate.

Worked example

x = 10, m = 1.5 + 0i (Wiscombe MIEV0)

Inputs: nParticleRe = 1.5, nParticleIm = 0, nHost = 1, diameterNm = 1.751e+3, wavelengthNm = 550

Result: 2.882

Reference: Wiscombe 1980, Appl. Opt. 19, 1505; BHMIE Appendix A

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#mie-scattering