Ghost Lab
What does the eye actually see reflected off a coated surface?
See what the eye sees. Render the ghost reflection of a lit scene on a coated surface and look at it from any angle. Brightness and colour come from the same transfer-matrix kernel as the TMM Simulator.
How it works
A coated surface reflects a fraction of every wavelength in the ambient scene, weighted by the coating's spectral and angular response. Rendering that physical reflection requires combining a scene radiance distribution with the surface reflectance spectrum at each pixel and applying a camera tone curve. The transfer-matrix method supplies the reflectance input for isotropic multilayer stacks.
Worked example
Bare glass vs single-layer n 1.22 vs 4-layer, D65, 30°
Shows the ghost ladder — 4.3 % → 0.01 % → 0.3 % photopic R.
Validation method, references and test-case results: /validation#ghost-lab