Drying Profile Planner
Check whether oven length, line speed, and temperature give the wet film enough dwell to dry, flagging under-cure when residence time falls below the diffusion estimate.
Validation: hand-checked example → /validation#drying-profile
Computes total dwell from oven length and line speed, splits across zones, and compares against a thickness-based Fickian diffusion estimate t ≈ thickness² / D_eff with D_eff = 1e-11 × exp((T_oven − T_BP)/30) m²/s — the brief Group 5 solvent-in-polymer midrange (1e-12 to 1e-10 m²/s, Zielinski & Hanley 1999). The margin ratio (dwell/required) flags severe under-cure below 0.5×, marginal between 0.5× and 1.0×. Air velocity, humidity, and skin formation are explicitly out of scope — the tool exists for triage and order-of-magnitude sizing before a coating trial.