Colour-Shift / Rainbow Index

How much does the reflected colour change with viewing angle?

Quantify the angular colour shift ('rainbow') of a multilayer stack as seen by a human observer, using CIE colorimetry.

How it works

Reflected spectra from thin films depend on the optical path length through each layer, which lengthens with increasing angle of incidence. Integrating the angle-dependent reflectance against a reference illuminant gives the reflected colour; the perceptual shift between two angles is quantified by the CIE ΔE* colour-difference metric in a uniform colour space such as CIELAB.

Worked example

CIEDE2000 Sharma pair 1

Inputs: lab1 = {"L":50,"a":2.6772,"b":-79.7751}, lab2 = {"L":50,"a":0,"b":-82.7485}

Result: 2.042 ΔE₀₀

Reference: Sharma, Wu & Dalal 2005 Color Res. Appl. 30, 21

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#colour-shift

Request accessOpen the interactive tool