All products
KM-404Available PFAS-free
Add NIR to External Material
ATO nanoparticle dispersion additive that can be incorporated into third-party materials to add NIR absorption. Bottom-up synthesised with haze <0.3%. Compatible with PVB, PU, and other host matrices for automotive and architectural glazing.
Refractive index rangen = 0.00–0.00
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-401–409
Specifications
Functions
NIR absorbing
Compatible substrates
PVBPUGlass
Processing methods
SPRAYDIP
Refractive index range
0.00–0.00
1.162.00
| Property | Value |
|---|---|
| Product code | KM-404 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 0.00–0.00 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | NIR absorbing |
| Compatible substrates | PVB, PU, Glass |
| Processing | SPRAY, DIP |
| Product block | KM-401–409 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Related case studies
Automotive Thermal<0.3%Haze (automotive grade)ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partnerAutomotive Thermal−9°CCabin temperature reductionCabin temperature reduced by 9°C with ATO glazing integrationAutomotive Thermal+16 kmRange extension (premium segment)16 km additional EV range through solar heat control glazing
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.