KM-203Available PFAS-free

Dual-Cure Antifouling

Dual-cure antifouling coating that achieves full cross-linking via combined UV and thermal cure. PFAS-free anti-smudge performance with WCA >100° on curved and complex substrates.

Refractive index rangen = 1.40–1.50
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeDual-cure
Product blockKM-201–203

Specifications

Functions

Antifouling

Compatible substrates

PCPMMAGlass

Processing methods

SPINDIPSPRAY

Refractive index range

1.40–1.50
1.162.00
PropertyValue
Product codeKM-203
Chemistry familySolvent UV-curable hybrid
Refractive index range1.40–1.50
Cure typeDual-cure
PFAS statusAvailable PFAS-free · fluorinated version available on request
FunctionsAntifouling
Compatible substratesPC, PMMA, Glass
ProcessingSPIN, DIP, SPRAY
Product blockKM-201–203
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.