All products
KM-104Available PFAS-free
Thermal NIR Absorbing
Thermal-curable NIR absorbing coating for direct glass application. Sol-gel formulation with ATO nanoparticles provides broadband NIR blocking. Suitable for high-temperature automotive glazing processes.
Refractive index rangen = 0.00–0.00
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-101–140
Specifications
Functions
NIR absorbing
Compatible substrates
Glass
Processing methods
SPINDIPSPRAY
Refractive index range
0.00–0.00
1.162.00
| Property | Value |
|---|---|
| Product code | KM-104 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 0.00–0.00 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | NIR absorbing |
| Compatible substrates | Glass |
| Processing | SPIN, DIP, SPRAY |
| Product block | KM-101–140 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.