All products
KM-058Available PFAS-free

UV ARHC

UV-curable hard coating with integrated anti-reflective functionality. Surface protection and reflection reduction in a single low-temperature cure.

Refractive index rangen = 1.30–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-051–059

Specifications

Functions

Hard coatingAnti-reflective

Compatible substrates

PETPCPMMATACGlass

Processing methods

SPINDIPROLLGRAVURESLOT DIE

Refractive index range

1.30–1.55
1.162.00
PropertyValue
Product codeKM-058
Chemistry familySolvent UV-curable hybrid
Refractive index range1.30–1.55
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsHard coating, Anti-reflective
Compatible substratesPET, PC, PMMA, TAC, Glass
ProcessingSPIN, DIP, ROLL, GRAVURE, SLOT DIE
Product blockKM-051–059
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us