All products
KM-056100% PFAS-free

UV HRI

UV-curable high refractive index coating, RI 1.65-1.95 for optical stack design, as a lower-temperature cure alternative to the thermal-cure KM-006.

Refractive index rangen = 1.65–1.95
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-051–059

Specifications

Functions

High RI

Compatible substrates

PETPCGlass

Processing methods

SPINDIPROLLSPRAY

Refractive index range

1.65–1.95
1.162.00
PropertyValue
Product codeKM-056
Chemistry familySolvent UV-curable hybrid
Refractive index range1.65–1.95
Cure typeUV
PFAS status100% PFAS-free
FunctionsHigh RI
Compatible substratesPET, PC, Glass
ProcessingSPIN, DIP, ROLL, SPRAY
Product blockKM-051–059
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us