All products
KM-051Available PFAS-free
UV HC
UV-curable sol-gel hard coating. Scratch-resistant surface protection with a low-temperature cure path for heat-sensitive substrates, as an alternative to the thermal-cure KM-008 and KM-025.
Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-051–059
Specifications
Functions
Hard coating
Compatible substrates
PETPCPMMATACGlass
Processing methods
SPINDIPROLLGRAVURESLOT DIE
Refractive index range
1.48–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-051 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.48–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Hard coating |
| Compatible substrates | PET, PC, PMMA, TAC, Glass |
| Processing | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Product block | KM-051–059 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.