All products
KM-044Available PFAS-free

Hydrophilic Coating

Sol-gel hydrophilic coating that promotes water sheeting for self-cleaning behaviour. UV-curable formulation for polymer and glass substrates.

Refractive index rangen = 1.45–1.55
1.162.00
Chemistry familySolvent sol-gel
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Hydrophilic

Compatible substrates

PETPCPMMAGlass

Processing methods

SPINDIPROLL

Refractive index range

1.45–1.55
1.162.00
PropertyValue
Product codeKM-044
Chemistry familySolvent sol-gel
Refractive index range1.45–1.55
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsHydrophilic
Compatible substratesPET, PC, PMMA, Glass
ProcessingSPIN, DIP, ROLL
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.