All products
KM-040Available PFAS-free

Multilayer Antireflection

Multi-layer anti-reflection stack utilising Kriya’s full RI platform (1.35–1.95) to achieve broadband residual reflectance below 0.15%. Validated on PET, PC, PMMA, and TAC substrates with transmission gains of 2–3.3%.

Refractive index rangen = 1.35–1.95
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeDual-cure
Product blockKM-001–040

Specifications

Functions

Anti-reflectiveMultilayer AR

Compatible substrates

PETPCPMMATACGlass

Processing methods

SPINDIPROLLGRAVURESLOT DIE

Refractive index range

1.35–1.95
1.162.00
PropertyValue
Product codeKM-040
Chemistry familySolvent UV-curable hybrid
Refractive index range1.35–1.95
Cure typeDual-cure
PFAS statusAvailable PFAS-free
FunctionsAnti-reflective, Multilayer AR
Compatible substratesPET, PC, PMMA, TAC, Glass
ProcessingSPIN, DIP, ROLL, GRAVURE, SLOT DIE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us