KM-035Available PFAS-free
AR + AF HC
Combined anti-reflective, antifouling, and hard coating in a UV-curable multi-layer or single-pot system. Addresses the three most common display surface requirements simultaneously.
Refractive index rangen = 1.35–1.60
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
Anti-reflectiveAntifoulingHard coating
Compatible substrates
PETPCPMMATAC
Processing methods
SPINDIPROLLGRAVURESLOT DIE
Refractive index range
1.35–1.60
1.162.00
| Property | Value |
|---|---|
| Product code | KM-035 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.35–1.60 |
| Cure type | UV |
| PFAS status | Available PFAS-free · fluorinated version available on request |
| Functions | Anti-reflective, Antifouling, Hard coating |
| Compatible substrates | PET, PC, PMMA, TAC |
| Processing | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample