Sol-gel precoat primer that improves adhesion of subsequent functional layers on polymer and glass substrates. UV-curable with broad substrate compatibility.

Refractive index rangen = 1.45–1.55
1.162.00
Chemistry familySolvent sol-gel
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Primer

Compatible substrates

PETPCPMMAGlass

Processing methods

SPINDIPROLL

Refractive index range

1.45–1.55
1.162.00
PropertyValue
Product codeKM-034
Chemistry familySolvent sol-gel
Refractive index range1.45–1.55
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsPrimer
Compatible substratesPET, PC, PMMA, Glass
ProcessingSPIN, DIP, ROLL
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.