Antisoiling on Plastic

UV-curable anti-soiling coating for plastic substrates including PET, PC, and PMMA. Provides self-cleaning properties on polymer surfaces where thermal cure is not feasible.

Refractive index rangen = 1.40–1.52
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Anti-soiling

Compatible substrates

PETPCPMMA

Processing methods

SPINDIPROLLGRAVURE

Refractive index range

1.40–1.52
1.162.00
PropertyValue
Product codeKM-031
Chemistry familySolvent UV-curable hybrid
Refractive index range1.40–1.52
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsAnti-soiling
Compatible substratesPET, PC, PMMA
ProcessingSPIN, DIP, ROLL, GRAVURE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.