All products
KM-022100% PFAS-free

Anti-Block HC

Hard coating with anti-blocking properties to prevent film-to-film adhesion during roll storage and handling. Essential for R2R production lines processing optical films.

Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Hard coating

Compatible substrates

PETTAC

Processing methods

ROLLGRAVURESLOT DIER2R

Refractive index range

1.48–1.55
1.162.00
PropertyValue
Product codeKM-022
Chemistry familySolvent UV-curable hybrid
Refractive index range1.48–1.55
Cure typeUV
PFAS status100% PFAS-free
FunctionsHard coating
Compatible substratesPET, TAC
ProcessingROLL, GRAVURE, SLOT DIE, R2R
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us