KM-017Available PFAS-free
AS AR
Combined antistatic and anti-reflective coating for display films. Reduces surface reflection while preventing electrostatic charge build-up during manufacturing and end-use.
Refractive index rangen = 1.35–1.60
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
AntistaticAnti-reflective
Compatible substrates
PETPCTAC
Processing methods
SPINDIPROLLGRAVURESLOT DIE
Refractive index range
1.35–1.60
1.162.00
| Property | Value |
|---|---|
| Product code | KM-017 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.35–1.60 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Antistatic, Anti-reflective |
| Compatible substrates | PET, PC, TAC |
| Processing | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |