All products
KM-013Available PFAS-free

1-Pot HC Thermal

Thermal-curable single-pot hard coating for substrates that cannot be exposed to UV light. Cures at temperatures from 80°C, making it suitable for heat-sensitive polymer lenses and pre-coated substrates.

Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-001–040

Specifications

Functions

Hard coating

Compatible substrates

GlassPCPMMACR-39

Processing methods

SPINDIPSPRAY

Refractive index range

1.45–1.50
1.162.00
PropertyValue
Product codeKM-013
Chemistry familyThermal-curable latex
Refractive index range1.45–1.50
Cure typeThermal
PFAS statusAvailable PFAS-free
FunctionsHard coating
Compatible substratesGlass, PC, PMMA, CR-39
ProcessingSPIN, DIP, SPRAY
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us