All products
KM-005Available PFAS-free

Low Refractive Index

Ultra-low refractive index coating reaching RI as low as 1.16 — the lowest available from any PFAS-free supplier globally. Overcoatable for multi-layer AR stacks. Proven to survive furnace tempering at 630°C and deliver 2.5–4.5× light guiding luminance improvement on glass substrates.

Refractive index rangen = 1.16–1.40
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-001–040

Specifications

Functions

Low RIAnti-reflective

Compatible substrates

GlassPETPCTAC

Processing methods

SPINDIPROLLSPRAY

Refractive index range

1.16–1.40
1.162.00
PropertyValue
Product codeKM-005
Chemistry familySolvent sol-gel
Refractive index range1.16–1.40
Cure typeThermal
PFAS statusAvailable PFAS-free
FunctionsLow RI, Anti-reflective
Compatible substratesGlass, PET, PC, TAC
ProcessingSPIN, DIP, ROLL, SPRAY
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.