All products
KM-004Available PFAS-free
NIR Absorbing
Near-infrared absorbing coating based on ATO nanoparticle dispersion. Blocks NIR radiation (800–2500 nm) while maintaining high visible light transmission. Designed for automotive glazing and solar heat control applications where reducing cabin temperature and AC load is critical.
Refractive index rangen = 0.00–0.00
1.162.00
Chemistry familySolvent sol-gel
Cure typeThermal
Product blockKM-001–040
Specifications
Functions
NIR absorbing
Compatible substrates
GlassPET
Processing methods
SPINDIPSPRAY
Refractive index range
0.00–0.00
1.162.00
| Property | Value |
|---|---|
| Product code | KM-004 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 0.00–0.00 |
| Cure type | Thermal |
| PFAS status | Available PFAS-free |
| Functions | NIR absorbing |
| Compatible substrates | Glass, PET |
| Processing | SPIN, DIP, SPRAY |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Related case studies
Automotive Thermal<0.3%Haze (automotive grade)ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partnerAutomotive Thermal−9°CCabin temperature reductionCabin temperature reduced by 9°C with ATO glazing integrationAutomotive Thermal+16 kmRange extension (premium segment)16 km additional EV range through solar heat control glazing
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.