KM-002100% PFAS-free
Antistatic
UV-curable antistatic coating providing surface resistivity in the 10⁹ Ohm/sq range. Prevents dust attraction and electrostatic discharge damage on display films and optical components. Proven at production scale, including 500,000 kg supplied as sole global supplier for PDP colour-filter applications.
Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
Antistatic
Compatible substrates
PETPCTACGlass
Processing methods
SPINDIPROLLGRAVURESLOT DIE
Refractive index range
1.48–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-002 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.48–1.55 |
| Cure type | UV |
| PFAS status | 100% PFAS-free |
| Functions | Antistatic |
| Compatible substrates | PET, PC, TAC, Glass |
| Processing | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |