← Back to all notes
R

Roel Huis in ‘t Veld

Director, Kriya Materials · Week of September 14, 2026

The PFAS-free deadline already passed. Now comes the hard part.

What food packaging can teach optical coatings about life after fluorine. For most of my industry, the PFAS restriction is still a future event. We talk about it in the conditional: when the universal restriction comes, when the derogations are settled, when the Commission finally publishes. Food-contact packaging does not have that luxury. Since 12 August 2026, when the Packaging and Packaging Waste Regulation entered into application, packaging containing PFAS above the defined limits may no longer be placed on the EU market. Pizza boxes, bakery paper, takeaway containers: for those, the deadline is not coming. It has passed. That is why I listened with more than professional curiosity to this week's European Coatings podcast, in which Jesús Palenzuela of the Spanish technology centre ITENE and Mireille Poelman, who coordinates the EU-funded Bio-SUSHY project, talked about what a PFAS-free functional coating on a fibre substrate actually has to do. The list is short and unforgiving: a water barrier, a grease barrier, a gas barrier, and afterwards the whole thing still has to go into the paper recycling stream. What struck me is how familiar this sounds from my own corner of the industry, which is optical and functional coatings on glass and plastic rather than on paper. Fluorine was never one property. It was a bundle. One chemistry gave you low surface energy, chemical inertness, a low refractive index and easy release, all at once, and the specifications our customers wrote over the past twenty years were quietly built around that bundle. A contact-angle number here, a slip requirement there, an index target that only a fluorinated polymer could reach at a sensible price. Take fluorine out and you do not replace one ingredient. You unbundle a specification and rebuild it from three or four different mechanisms. I wrote about one such rebuild last year in PCI, on replacing fluorinated antistatic additives with antimony-doped tin oxide. The chemistry was the easy part of that story. The hard part was that a substitute has to be argued into a specification that was never written with it in mind. I say this as someone whose own catalogue still contains fluorinated chemistry where nothing else yet meets the specification, so I am not preaching from a clean sheet. Two things in the podcast deserve attention from anyone who coats anything. The first is that both speakers talk about application methods as much as about materials: plasma deposition as a solvent-free route, electrostatic dry powder coating as a zero-solvent one. This matches my experience exactly. Fluorine-free is not a formulation swap, it is a process redesign. The alternative chemistry usually wants a different cure, a different thickness window, sometimes a different line speed, and the customer's qualification protocol has to be run again from the beginning. A specialty SME feels this in one very specific place: the qualification queue. Every replacement product goes through the same long cycle of samples, pilot runs and audits as a new product, because to the customer it is one. The second is Poelman's use of the Commission's Safe and Sustainable by Design framework and of computational modelling to predict barrier performance on a rough fibre surface before anything is coated. Ten years ago that would have been an academic exercise. Today it is how a small consortium keeps up with a deadline. This is the convergence I keep returning to in G-Force Disruption: regulation sets the clock, but simulation, cheap compute and new deposition tools are what let a team of a few dozen people move at the speed the clock demands. Meanwhile the big one, the universal restriction under REACH, grinds on. SEAC's draft opinion went out for consultation in March, the consultation closed in May, and a final opinion is expected around the end of this year, after which the Commission has to turn it into law and the member states have to vote. Nothing about that timetable moved this week. That is precisely my point. The parts of our industry that are already living after fluorine are not the ones waiting for Helsinki. They are the ones whose customers stopped waiting. If you make coatings and you have not yet had a customer ask for a fluorine-free version of something they have bought from you for a decade, you will. My advice, from someone who has been through it more than once, is to start with the specification, not the formulation. Find out which numbers on that sheet are real requirements and which are fossils of the old chemistry. You will be surprised how many are fossils. Sources European Coatings, 17 Aug 2026 — EU packaging regulation enters into force: PFAS restrictions in food-contact packaging now in effect — https://www.european-coatings.com/news/legislation/eu-packaging-regulation-enters-into-force-pfas-restrictions-in-food-contact-packaging-now-in-effect/ European Coatings, 9 Sep 2026 — EC Podcast: Functional and PFAS-free food packaging coatings (Palenzuela, ITENE; Poelman, Bio-SUSHY) — https://www.european-coatings.com/news/application-areas/ec-podcast-functional-and-pfas-free-food-packaging-coatings/ PCI Magazine, 4 Mar 2025 — Escaping the PFAS Ban (Roel Huis in 't Veld) — https://www.pcimag.com/articles/113301-escaping-the-pfas-ban Deloitte, 7 Apr 2026 — SEAC draft opinion on the universal PFAS restriction: consultation to 25 May 2026, final opinion expected end 2026 — https://www.deloitte.com/at/de/services/tax/blogs/2026/breaking-news-chemicals-agency-eu-restrictions-pfas.html