Todos los casos de estudio
Pantallas — ULR

La composición de nanopartículas ARAF alcanza 0,3 veces el nivel de reflexión de referencia

Un fabricante japonés líder de películas AR

Indicadores clave

0.3×Reflexión frente a referencia
95.6%Transmisión total
0.5%Turbidez
PassAntisuciedad (borrado de marcador)

01

El desafío

The AR film manufacturer needed a nanoparticle ARAF composition that could achieve ultra-low reflection significantly below their internal reference level, while maintaining acceptable haze and anti-smudge properties for premium display applications.

02

Nuestro enfoque

Kriya developed ARAF nanoparticle compositions in two particle sizes (50 nm for low reflection, 75 nm for super-low reflection). Multiple formulation versions were tested at the manufacturer’s facility against their internal reference samples, measuring reflection, haze, transmission, steel wool abrasion, and anti-smudge performance.

03

El resultado

The 75 nm super-low-reflection variant achieved reflection at 0.3× the reference level with 95.6% total transmission and 0.5% haze. The 50 nm low-reflection variant achieved 0.7× reference reflection with improved abrasion resistance. Both variants passed anti-smudge (fingerprint and marker wipe-off) testing.

Por qué Kriya

Kriya’s tuneable nanoparticle platform enables precise control over the reflection–abrasion trade-off, allowing customers to select the optimal balance for their application.

Indicadores clave

0.3×Reflexión frente a referencia
95.6%Transmisión total
0.5%Turbidez
PassAntisuciedad (borrado de marcador)

Productos utilizados

Aplicación relacionada

Displays — ULR →

Discutir una aplicación similar

Nuestro equipo técnico puede ayudarle a evaluar si este enfoque es aplicable a sus requisitos específicos.

Iniciar una conversación