All products
KM-702Available PFAS-free
UV 100% HC
UV-curable 100% solids hard coating variant optimised for specific viscosity and cure speed requirements in high-volume production. Complements KM-701 for different processing windows.
Refractive index rangen = 1.50–1.55
1.162.00
Chemistry family100% solids UV-curable
Cure typeUV
Product blockKM-700–704
Specifications
Functions
Hard coating
Compatible substrates
PETPC
Processing methods
R2RNILSLOT DIE
Refractive index range
1.50–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-702 |
| Chemistry family | 100% solids UV-curable |
| Refractive index range | 1.50–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Hard coating |
| Compatible substrates | PET, PC |
| Processing | R2R, NIL, SLOT DIE |
| Product block | KM-700–704 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related applications
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.