All products
KM-309100% PFAS-free

100% AG Hard Coat

Solvent-free 100% solids UV-curable hard coating with anti-glare functionality. Provides glare reduction and surface protection in a zero-VOC formulation compatible with R2R manufacturing.

Refractive index rangen = 1.48–1.55
1.162.00
Chemistry family100% solids UV-curable
Cure typeUV
Product blockKM-301–309

Specifications

Functions

Hard coatingAnti-glare

Compatible substrates

PETPCPMMA

Processing methods

R2RNILSLOT DIE

Refractive index range

1.48–1.55
1.162.00
PropertyValue
Product codeKM-309
Chemistry family100% solids UV-curable
Refractive index range1.48–1.55
Cure typeUV
PFAS status100% PFAS-free
FunctionsHard coating, Anti-glare
Compatible substratesPET, PC, PMMA
ProcessingR2R, NIL, SLOT DIE
Product blockKM-301–309
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.