All products
KM-301Available PFAS-free
100% Solids HC
Solvent-free 100% solids UV-curable hard coating for high-throughput R2R and NIL processing. Zero VOC emissions. Enables precise nanostructure replication for waveguide gratings and metalens patterns.
Refractive index rangen = 1.50–1.55
1.162.00
Chemistry family100% solids UV-curable
Cure typeUV
Product blockKM-301–309
Specifications
Functions
Hard coating
Compatible substrates
PETPCPMMAGlass
Processing methods
R2RNILSCREEN PRINTINGSLOT DIE
Refractive index range
1.50–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-301 |
| Chemistry family | 100% solids UV-curable |
| Refractive index range | 1.50–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Hard coating |
| Compatible substrates | PET, PC, PMMA, Glass |
| Processing | R2R, NIL, SCREEN PRINTING, SLOT DIE |
| Product block | KM-301–309 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.