All products
KM-140Available PFAS-free

Thermal Anti-Corrosion

Thermal-curable anti-corrosion coating for metal and glass substrates exposed to harsh environments. Provides barrier protection against moisture and chemical attack.

Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-101–140

Specifications

Functions

Anti-corrosion

Compatible substrates

GlassMetal

Processing methods

SPINDIPSPRAY

Refractive index range

1.45–1.50
1.162.00
PropertyValue
Product codeKM-140
Chemistry familyThermal-curable latex
Refractive index range1.45–1.50
Cure typeThermal
PFAS statusAvailable PFAS-free
FunctionsAnti-corrosion
Compatible substratesGlass, Metal
ProcessingSPIN, DIP, SPRAY
Product blockKM-101–140
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us