All products
KM-130100% PFAS-free

Thermal Anti-Soiling

Thermal-curable anti-soiling coating for architectural glass and solar panels. Reduces surface contamination and maintenance frequency. Compatible with high-temperature glass processing lines.

Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-101–140

Specifications

Functions

Anti-soiling

Compatible substrates

Glass

Processing methods

SPINDIPSPRAY

Refractive index range

1.45–1.50
1.162.00
PropertyValue
Product codeKM-130
Chemistry familyThermal-curable latex
Refractive index range1.45–1.50
Cure typeThermal
PFAS status100% PFAS-free
FunctionsAnti-soiling
Compatible substratesGlass
ProcessingSPIN, DIP, SPRAY
Product blockKM-101–140
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.