All products
KM-103100% PFAS-free

Thermal Hydrophobic

Thermal-curable hydrophobic coating providing high water contact angles for water-repellent surfaces. PFAS-free water-shedding functionality for automotive, architectural, and display applications.

Refractive index rangen = 1.45–1.50
1.162.00
Chemistry familyThermal-curable latex
Cure typeThermal
Product blockKM-101–140

Specifications

Functions

Hydrophobic

Compatible substrates

GlassPCPMMA

Processing methods

SPINDIPSPRAY

Refractive index range

1.45–1.50
1.162.00
PropertyValue
Product codeKM-103
Chemistry familyThermal-curable latex
Refractive index range1.45–1.50
Cure typeThermal
PFAS status100% PFAS-free
FunctionsHydrophobic
Compatible substratesGlass, PC, PMMA
ProcessingSPIN, DIP, SPRAY
Product blockKM-101–140
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.