All products
KM-044Available PFAS-free
Hydrophilic Coating
Sol-gel hydrophilic coating that promotes water sheeting for self-cleaning behaviour. UV-curable formulation for polymer and glass substrates.
Refractive index rangen = 1.45–1.55
1.162.00
Chemistry familySolvent sol-gel
Cure typeUV
Product blockKM-001–040
Specifications
Functions
Hydrophilic
Compatible substrates
PETPCPMMAGlass
Processing methods
SPINDIPROLL
Refractive index range
1.45–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-044 |
| Chemistry family | Solvent sol-gel |
| Refractive index range | 1.45–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free |
| Functions | Hydrophilic |
| Compatible substrates | PET, PC, PMMA, Glass |
| Processing | SPIN, DIP, ROLL |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.