All products
KM-040Available PFAS-free
Multilayer Antireflection
Multi-layer anti-reflection stack utilising Kriya’s full RI platform (1.35–1.95) to achieve broadband residual reflectance below 0.15%. Validated on PET, PC, PMMA, and TAC substrates with transmission gains of 2–3.3%.
Refractive index rangen = 1.35–1.95
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeDual-cure
Product blockKM-001–040
Specifications
Functions
Anti-reflectiveMultilayer AR
Compatible substrates
PETPCPMMATACGlass
Processing methods
SPINDIPROLLGRAVURESLOT DIE
Refractive index range
1.35–1.95
1.162.00
| Property | Value |
|---|---|
| Product code | KM-040 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.35–1.95 |
| Cure type | Dual-cure |
| PFAS status | Available PFAS-free |
| Functions | Anti-reflective, Multilayer AR |
| Compatible substrates | PET, PC, PMMA, TAC, Glass |
| Processing | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Related case studies
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stackDisplays — ULR0.3×Reflection vs referenceARAF nanoparticle composition achieves 0.3× reference reflection level
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.