All products
KM-036Available PFAS-free

Antifingerprint

Dedicated anti-fingerprint coating optimised for touch-interactive surfaces. PFAS-free formulation achieves water contact angle >100° with exceptional fingerprint visibility reduction and easy wipe-off.

Refractive index rangen = 1.40–1.50
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040

Specifications

Functions

Anti-smudge

Compatible substrates

PETPCPMMAGlass

Processing methods

SPINDIPROLLGRAVURE

Refractive index range

1.40–1.50
1.162.00
PropertyValue
Product codeKM-036
Chemistry familySolvent UV-curable hybrid
Refractive index range1.40–1.50
Cure typeUV
PFAS statusAvailable PFAS-free
FunctionsAnti-smudge
Compatible substratesPET, PC, PMMA, Glass
ProcessingSPIN, DIP, ROLL, GRAVURE
Product blockKM-001–040
Batch sizesFrom 40 kg sample to production scale
Shelf life6 months (unopened)
QualityISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch.

Request a sample

Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.

Contact us