All products
KM-032Available PFAS-free
AS AF HC UV Weatherable
Four-function UV-curable coating: antistatic, antifouling, hard coating, and UV weatherability. Designed for demanding outdoor display applications that require multiple protective functions in minimal layers.
Refractive index rangen = 1.48–1.55
1.162.00
Chemistry familySolvent UV-curable hybrid
Cure typeUV
Product blockKM-001–040
Specifications
Functions
AntistaticAntifoulingHard coating
Compatible substrates
PETPCPMMA
Processing methods
SPINDIPROLLGRAVURE
Refractive index range
1.48–1.55
1.162.00
| Property | Value |
|---|---|
| Product code | KM-032 |
| Chemistry family | Solvent UV-curable hybrid |
| Refractive index range | 1.48–1.55 |
| Cure type | UV |
| PFAS status | Available PFAS-free · fluorinated version available on request |
| Functions | Antistatic, Antifouling, Hard coating |
| Compatible substrates | PET, PC, PMMA |
| Processing | SPIN, DIP, ROLL, GRAVURE |
| Product block | KM-001–040 |
| Batch sizes | From 40 kg sample to production scale |
| Shelf life | 6 months (unopened) |
| Quality | ISO 9001:2015 certified. Filtered to 0.8 µm. Up to 10 CTQ parameters per batch. |
Request a sample
Available from 40 kg sample batches. Every batch filtered to 0.8 µm and tested on up to 10 critical-to-quality parameters.